Duplex 2205 plates are available for enquiry as stainless steel flat products. A duplex stainless steel combining higher strength than common austenitic grades with improved resistance to chloride stress corrosion cracking. This grade is specified by its material standard and UNS designation; the right finish and tolerance depend on fabrication and service conditions.
For duplex 2205 plates, send thickness, width and length, grade designation (S32205 or S31803), finish, quantity and destination. Confirm size and testing requirements before ordering; weld procedures and grade substitution require engineering review.
Quick specifications
| Property | Specification / ordering detail |
|---|---|
| Material standard | ASTM A240 / ASME SA240 (flat-rolled stainless steel) |
| Grades covered | Duplex 2205: specify UNS S32205 or S31803; dual certification only when the material certificate explicitly supports both. |
| Thickness range | Specify thickness; stock range on request |
| Width / size range | Specify width; availability on request |
| Length | Cut length on request |
| Finish options | Mill or processed finish; polished/bright finishes only where feasible in the quoted thickness |
| Form | Heavy flat plates; state cut dimensions and edge condition |
Equivalent designations
| System | Designation |
|---|---|
| UNS | S32205 (also S31803) |
| Werkstoff Nr. | 1.4462 |
| JIS | SUS 329J3L |
| EN | 1.4462 |
| BS | 318S13 |
Chemical composition
Published typical values by Outokumpu, mass %. A dash means no typical value stated in the cited summary, not zero or an ASTM limit. Request the actual MTC for supplied material.
| Grade / basis | C | Mn | Si | P | S | Cr | Ni | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| Duplex 2205 typical (%) | 0.02 | — | — | — | — | 22.4 | 5.7 | 3.1 | 0.17 |
Mechanical properties
ASTM A240 minimums for plate, sheet and strip, annealed condition. Hardness is not stated in this cited summary; check the applicable purchase standard and MTC.
| Grade / ASTM A240 minima | Tensile (MPa) | 0.2% yield (MPa) | Elongation (%) | Hardness |
|---|---|---|---|---|
| Duplex 2205 | 655 | 450 | 25 | — |
Source: Outokumpu Forta DX 2205 datasheet ↗. Values vary by product form, condition and standard; not a substitute for the material certificate.
What these numbers mean for a buyer
The chemistry row shows a published typical production example, not min/max acceptance ranges. The mechanical row shows minimum values from the cited ASTM A240 summary, not guaranteed results for any individual coil or plate. Review the exact heat number and measured results on the supplied EN 10204 3.1 mill certificate. UNS identifies the alloy; thickness, finish and dimensional tolerances must still be specified separately.
Practical ordering checklist
- Material grade and UNS, plus whether dual certification is required.
- ASTM/ASME or EN standard and revision required by the project.
- Thickness, width and cut length, plus tolerances and edge condition.
- Finish, quantity, delivery destination and packing requirements.
- MTC, inspection, surface testing and any project-specific corrosion test.
Forms and finishes
Plates are flat-rolled forms, but ordering dimensions and feasible finishes vary by thickness, route and grade. Confirm the requested finish, tolerances and certificate for this specific plate before quoting.
Typical applications
Chemical processing, marine systems, heat exchangers and demanding fabrication. Engineering selection must account for the actual fluid, temperature, environment and code.
Related products
- SS 304 Sheets
- SS 316 Sheets
- SS 304 Plates
- SS 316 Plates